Customization: | Available |
---|---|
Carrier: | PVC |
Certification: | ISO |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
PVC H-70 protective layer plastic particles | |||||||
Test project | unit | performance index | standard | ||||
1 | tensile strength | MPa | ≥15 | GB/T1040.3-2006 | |||
2 | elongation at break | % | ≥180 | GB/T2951.12-2008 | |||
3 | Impact brittleness test | test temperature | ºC | -20 | GB/T5470-2008 | ||
Impact brittleness performance | ------ | 15/30 | |||||
4 | 200 ºC thermal stability time | min | ≥60 | GB/T8815-2008 | |||
6 | hardness | Shore A | 83±2 | GB/T2411-2008 | |||
7 | density | g/cm3 | ≤1.4 | GB/T1033.1-2008 | |||
8 | Oxygen Index | % | / | GB/T2406.2-2009 | |||
9 | Hot deformation at 120 ºC/1h | % | / | GB/T8815-2008 | |||
10 | Thermal shock at 150 ºC/1H | / | / | GB/T5023.1-2008 | |||
11 | dielectric strength | MV/m | ≥20 | GB/T1408-2016 | |||
12 | Volume resistivity at 20 ºC | Ω·m | ≥1.0*1012 | GB/T1410-2006 | |||
13 | heat aging property | test temperature | ºC | 100±2 | GB/T8815-2008 | ||
Test time | h | 168 | GB/T8815-2008 | ||||
Tensile strength after aging | MPa | ≥15 | GB/T8815-2008 | ||||
Maximum rate of change in tensile strength | % | ±20 | GB/T8815-2008 | ||||
Elongation at break after aging | % | ≥180 | GB/T8815-2008 | ||||
Max change of elongation at break | % | ±20 | GB/T8815-2008 | ||||
Quality loss due to thermal aging | Experimental conditions | ------ | / | GB/T8815-2008 | |||
Mass loss | g/cm2 | ≤20 | GB/T2951.31-2008 | ||||
14 | environmental requirements | According to customer requirements |